Question: What percentage of powered ferrosilicon is mixed with sodium silicate bonded sand in Nishiyama process?

Options

A : 1%

B : 2%

C : 3%

D : 4%

Click to view Correct Answer

Next

Casting Types Cores more questions

What is the amount of loss suffered by an induction....

What is the amount of sea coal needed in cast....

Pitch maybe used up to what percent?

The tolerances on the cross-section of the test specimens shall....

The tolerances on the cross-section of the test specimens shall....

The ramp input is applied to a unity feedback system....

In magnesium alloys, what is the bentonite percentage composition?

In dry sand moulding of steel casting, what is the....

What percent of PAR is captured by plants?

It results in the failure of concrete made from the....

Chemical Engineering Basics - Part 1 more Online Exam Quiz

Casting Squeeze Casting

Casting Steps Involved Making Mold

Casting Test

Casting Testing Core Sands

Casting Testing Mechanical Properties

Casting Types Molds

Casting Types Pattern

Casting Types Risers

Casting Vacuum Die Casting

Casting Venting Moulds